CF-Andrew Park 2-LR 940203 (2) DI~MIX
CONCRETE MIX DESIGN
CLIENT :
PROJECT :
LOCATION :
Rodman Excavating DATE:_ 2/03/94
Andrew Brown Jr. Community Park / Phase. II
Coppell, Texas
MIX 9 0504
DESIGN SPECIFICATIONS: 5.0 sack- WRA/AEA
28 Day Strength:
Cement Content :
Fly Ash Content :
Slump :
Aggregate Size :
Water Reducing Admixture:
Air Entraining Admixture:
3000 psi
5.0 sack
00.0 %
3-5 inch
1"-%4 crushed stone
ASTM C494 Type A or D
ASTM C260 4-7 %
MATERIALS: One Cubic Yard Weights (SSD)
AB S. VOLUME
Cement ASTM C150
Fly Ash ASTM C618
Coarse Aggregate
Fine Aggregate
Water
Admixture ASTM C494
Admixture ASTM C260
470 lbs. 2.391
00 lbs.
1840 lbs. 11.212
1326 lbs. 8.176
29.0 gals 3.871
14.0 oz/yd
2.00 oz/yd 1.350
27.000 cf
PLEASE NOTE
ASTM C94 Standard Speciffcations.for Ready Mix Concrete states as
follows; "When the concrete strength is used as a basis for
acceptance, the manufacturer shall be entitled to copies of test
reports.. The individual who samples and tests concrete must be
certified ACI Level
To assist in the quality control and quality assurance of your
mix, provide reports on a timely basis.
To insure proper design order by MIX ~ 0504
Manager
Date
REDI-MIX, Inc.
GENERAL OFFICE/1445 MaaAr~hur Drive, Suite 136, Carrollton, Texas 75007