SC-Coppell HS-LR000301FUGRO SOUTH, INC.
2880 Virgo Lane; Dallas, Texas 75229
Ph (972) 484-8301; Fax (972) 620-7328
COMPRESSIVE STRENGTH OF MORTAR CUBES
CLIENT: Coppell lSD, c/o Dal - Mac Construction Co. Report Date: March 1, 2000
PROJECT: Coppell High School, High School Expansion Project No.: 0791-2208
Coppell, Texas
SAMPLE DATE: February 21, 2000
Contractor: Skinner Masonry
Method of Test: ASTM C-109
Sample Location: Cl.5-CA, Area c, Tier 1
Time Batched: 2:45 Time Sampled: 3:05
Results / Remarks: Type N
SAMPLE AGE DATE AREA APPLIED COMPRESSIVE REQUIRED
NUMBER TESTED LOAD STRENGTH STRENGTH
(days) (sq. in.) (lbs.) (psi) (psi/days)
CHC I 7 02/28/00 4.0 2670 670 750/28
CHC 2 7 02/28/00 4.0 2890 720
CHC 3 7 02/28/00 4.0 3000 750
CHC 4 28 03/20/00 4.0
CHC 5 28 03/20/00 4.0
CHC 6 28 03/20/00 4.0
Remarks:
Mike Flute
Technician FUGRO SOUTH INC.
Reviewed By:
SMH/rm
Distribution: DaI-Mac Construction - Damon Norman
City of Coppell - Larry Davis
Coppell lSD - Mickey Harper
SHW Group - Joe Craddock
SHW Group - Mike Elmore
JRJ Paving - Jeff Williford